I-elektrode electrode iya kuba yigrafu ephezulu yobushushu obuqhubayo, eyona nto iphambili kwi-Petroleum Coke, i-Car Coke njenge-filler, i-coal tha i-binder. Sivelisa i-elektroder electrodes kunye neengoloni kubo. Igrafu elektroniki iphawuleka ngokuxhathiswa okuphantsi, ukuqhubela kombane kunye nokuphumelela okuphezulu, ukunyangwa okuphezulu, oko kukwahlulwa kwi-elektronerrode ye-elektroniki, amandla aphezulu Igrafu electrode kunye ne-Ultra enkulu ye-Eltraderrode ye-elektroniki.
1.Ukuhlala kombane
I-2. Ukuxinana okuphezulu
3. Ukuqhutywa kombane okuhle
I-4. Ukuphakama okuphezulu kwe-oxidation
5. Ukuchaneka komatshini
I-6. I-SHFUR esezantsi kunye ne-ash esezantsi, ayiniki ityholo lesibini lesibini
Igrafu eleckiterodes isetyenziswa ikakhulu kwizikweni zeLadle, i-Arc ye-Arc yombane ye-ARC, iPhosphor yezixhobo, ye-phosphor ye-phosphor, iZiko leSilicon. Okwangoku zezona mpahla zifumanekayo ezinamanqanaba aphezulu okuqhutywa kombane kunye nokwazi ukuxhasa amanqanaba aphezulu obushushu oveliswe kule ndawo ye-HP & UHP I-OHPRODE Ecke kwi-elektrode ye-elektrode. Igrafu eleckiterodes ikwasetyenziselwa ukucoca intsimbi kwi-ladle yezixhobo kunye nezinye iinkqubo zokunyibilika.
I-1.Inzelwa kakuhle kwiziko le-ARC le-ARC
2.Kaloku isithando somlilo; iziko lokuchasana;
3.Ke ukuveliswa kweemveliso zegrafine;
4.Ke ukuveliswa kweemveliso zegrafu ezenziwe ngemizobo;
5.Unokuthi usetyenziselwe izixhobo zokuhambisa;
6. Ukuveliswa kweemveliso ezinomzobo omiweyo;
Igama | Iyunithi | Ububanzi beNgoma | ||||||
Uhp ultra-high righ-high | Hp superstrong | I-RP eqhelekileyo yamandla | ||||||
≤φ400 | ≥φ450 | ≤φ400 | ≥φ450 | ≤φ300 | ≥φ350 | |||
Ukuxhathisa | I-electrode | Ω ω · m | ≤5.5 | ≤6.5 | ≤8.5 | |||
Ingono | ≤4.5 | ≤5.5 | ≤6.5 | |||||
Amandla e-flexual | I-electrode | Mpa | ≥11.0 | ≥10.5 | ≥9.8 | ≥8.5 | ≥7.0 | |
Ingono | ≥20.0 | ≥16.0 | ≥15.0 | |||||
I-Elastic modyul | I-electrode | I-GPA | ≤14.0 | ≤12.0 | ≤9.3 | |||
Ingono | ≤18.0 | ≤16.0 | ≤14.0 | |||||
Ukuxinana | I-electrode | g / cm3 | ≥1.66 | ≥1.67 | ≥1.62 | 1.6 | ≥1.53 | ≥1.52 |
Ingono | ≥1.75 | ≥1.73 | ≥1.69 | |||||
Ukusebenza kolwando lwe-shirmal | I-electrode | I-10-6 / ℃ | ≤1.5 | ≤2.4 | ≤2.9 | |||
Ingono | ≤1.4 | ≤2.2 | ≤2.8 | |||||
I-ash | % | ≤0.3 | ≤0.3 | ≤0.5 |